Tris(trimethylsilyl)phosphate (TMSP, CAS 10497‑05‑9) is organosilicon phosphate ester high‑voltage electrolyte additive. It forms robust CEI film on high‑voltage cathode, scavenges HF and trace moisture, suppresses metal dissolution and improves high voltage cycling performance of lithium ion batteries.
Chemical Name: Tris(trimethylsilyl)phosphate
Synonyms: TMSP / TMSPa, Tris (trimethylsilyl) orthophosphate
CAS NO: 10497‑05‑9
EINECS Number: 234‑028‑1
Formula: C₉H₂₇O₄PSi₃
Molecular Weight: 314.54 g/mol
Product Type: Lithium‑ion battery electrolyte high‑voltage CEI film‑forming additive, organosilicon fine chemical, HF scavenger
Product Grade: Battery Electronic Grade / Research Laboratory Grade
|
Item |
Specification |
|
Appearance |
Colorless to pale yellow transparent liquid |
|
Purity |
≥99.0 % |
|
Acidity (as HF) |
≤15 ppm |
|
Chloride Ion (Cl⁻) |
≤2 ppm |
|
Metal Impurity (Na, K, Fe, Ni etc.) |
≤1 ppm each |
|
Melting Point |
3–4 ℃ |
|
Boiling Point |
228‑229 ℃ |
|
Density (25 ℃, g/cm3) |
0.945 |
|
Refractive Index |
1.409 |
Description:
Tris(trimethylsilyl)phosphate (TMSP, CAS 10497‑05‑9) is an organosilicon phosphate ester compound. It is a high‑voltage cathode electrolyte additive, preferentially oxidized on high‑nickel, LNMO cathode surface to form dense, P‑Si‑rich CEI (Cathode Electrolyte Interphase) film.
TMSP also acts as an effective HF / moisture scavenger in electrolyte system, it consumes trace water and hydrofluoric acid impurities, suppresses metal ion leaching from cathode material, reduces electrolyte continuous oxidative decomposition at high voltage. It is colorless to pale yellow transparent liquid at room temperature, extremely sensitive to moisture, must be strictly protected from water. Battery‑grade TMSP requires rigorous control of moisture, free acid and metal impurities.
Core advantages: Forms stable high‑voltage CEI film, captures HF and trace water, inhibits cathode metal dissolution, improves high‑voltage cycle & high‑temperature storage performance, suppresses battery self‑discharge, zero ozone depletion potential.
Application:
High voltage CEI forming additive for NCM high nickel, LNMO cathode lithium‑ion batteries, widely used in power battery and high energy density battery electrolyte formulations. Typical dosage: 0.2 ~ 2.0 wt%.
Removes trace moisture and HF impurity, reduce electrolyte aging and cathode corrosion.
Silylation reagent and phosphorus‑containing building block for organosilicon synthesis.
Model high‑voltage additive for cathode‑electrolyte interphase research.
Packaging: 100g /500g /1kg /5kg nitrogen‑sealed stainless‑steel drum / amber glass bottle; sealed under nitrogen inert atmosphere.
Storage: Store in cool, dry, dark professional chemical warehouse. Recommended long‑term storage temperature: 2‑8 ℃. Keep container tightly sealed under nitrogen protection, strictly prevent moisture ingress. Keep away from heat and direct sunlight.
Shelf Life: 12 months for unopened nitrogen sealed package under recommended storage conditions. Once opened, consume rapidly under inert gas environment.